How would you take a mould from this?


Author
Message
doormatt
doormatt
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 67
Hi all first post here so hope i'm not posting in the wrong section, i've got a part i want to take a mould of to make carbon fibre copies of it. As you can see it's quite an awkward shape, how would you lot take a mould? 2 piece split mould if so would you go down the middle? 

 http://www.talkcomposites.com/Uploads/Images/146de6ac-7cbb-4916-b479-bf8f.JPG
http://www.talkcomposites.com/Uploads/Images/fd5c2160-c87a-4c25-9c84-89b8.JPG
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I'm not sure I see why it couldn't be a one piece mould... 