Group: Moderators
Posts: 226,
Visits: 334
|
Should be able to get that to pull down with a little thought,
main problems ive had with bridging in a part like that is mostly due to the excess/off part carbon clamping and not sliding.
you always get really good vac on the flats, these clamp first then stop the cloth from seating in the corners, ive found if you cut back as much of the over hang/ off part cloth as you can it will pull in.
|