Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Silicone intensifiers
Silicone intensifiers
Post Reply
Like
3
Silicone intensifiers
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Darren
Darren
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 54,
Visits: 916
Has any one used/made intensifiers?
And can they be used with infusion?
Im having real trouble getting my stack right down in to a small sharp 90 degree bend, it only bridges a very small amount…
Reply
Like
3
Reply
Darren
Darren
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 54,
Visits: 916
VVS (28/10/2015)
Should be able to get that to pull down with a little thought,
main problems ive had with bridging in a part like that is mostly due to the excess/off part carbon clamping and not sliding.
you always get really good vac on the flats, these clamp first then stop the cloth from seating in the corners, ive found if you cut back as much of the over hang/ off part cloth as you can it will pull in.
I cut off as much excess as i could and the end result was perfect..
Thanks
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Silicone intensifiers
Darren
-
10 Years Ago
Yeh you can use a silicone intensifier with infusion, just place it on top of your flow mesh.
Hanaldo
-
10 Years Ago
Does EC sell a silicone suitable for making intensifiers? And what is the best way to go about...
Darren
-
10 Years Ago
Should be able to get that to pull down with a little thought, main problems ive had with bridging...
VVS
-
10 Years Ago
[quote][b]VVS (28/10/2015)[/b][hr]Should be able to get that to pull down with a little thought,...
Darren
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search