Has any one used/made intensifiers?

And can they be used with infusion?

Im having real trouble getting my stack right down in to a small sharp 90 degree bend, it only bridges a very small amount…






Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh you can use a silicone intensifier with infusion, just place it on top of your flow mesh. 
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Does EC sell a silicone suitable for making intensifiers?

And what is the best way to go about making then? sheet wax in the mould then pour silicone in?