First off can i say none of this would happen if it it wasn't for Paul, Matt and the guys at Easy Composites,
to say you couldn't meet a nicer, more helpful, informative, interested in your project, etc, etc. bunch of people.
Paul and Matt have bent over backwards to help me and thanks have to be said.

I first went to EC at the old building to pick up a skinning kit to skin the header tank on my road bike and ended up making a  rea rseat cover

can be seen in the picture


This was a bad idea and has sent me down the road of composite hell, lol
I started rebuilding an old gsxr 400 race bike and decided to replace all the old uv damaged panels in CF.

first part was the air box so I got to work.

will use tank as top of box


my first play with wax sheet and filleting wax


box fitted to bike


  
Edited 11 Years Ago by VVS
Reply
VVS
VVS
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Not sure about the sniffer as i believe they don't work with the very small leaks.

As you can read i had some problems with micro vac leaks on the nose cone.
I think its mostly down to me being as deaf as a mole so i will have to live with them.

Nose cone.

I have to say i was not looking forward to laying this up, i needed to put cuts in the cloth and the bowl shape made it hard to lay everything in.
Using peel ply i made templates for the CF and then having laid each piece i tacked them together with the spay glue.
I aimed to infuse from the centre of the part but found the task of taping spiral all the way around the perimeter a daunting task so went with 
the easier option of feeding one side to the other.

First piece of CF in place.
You can see also the join in the mould.
    

The other 4 sides in place.
Looking good so far.
  

Finally part under vacuum, Cheers Paul.
Two more layers of CF plus peel ply and mesh and waiting resin.
 

Part way through the infusion.


Further on in the infusion,
i was panicking that the resin would not reach the two outer edges but all was ok.
 

Infusion finished Smile

Finished untrimmed part,
Im a very happy man.




There are a couple of VERY small marks and two tiny voids but its a virgin part from a virgin mould,
everything im doing is a first time part so im ok with minor after work.

Chris.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
VVS - 11 Years Ago
VVS - 11 Years Ago
Warren (Staff) - 11 Years Ago
davro - 11 Years Ago
VVS - 11 Years Ago
VVS - 11 Years Ago
Hanaldo - 11 Years Ago
redeye - 11 Years Ago
VVS - 11 Years Ago
scottracing - 11 Years Ago
Matt (Staff) - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
VVS - 11 Years Ago
davro - 11 Years Ago
Hanaldo - 11 Years Ago
VVS - 11 Years Ago
Warren (Staff) - 11 Years Ago
VVS - 11 Years Ago
matthieutje65 - 11 Years Ago
VVS - 11 Years Ago
Hanaldo - 11 Years Ago
VVS - 11 Years Ago
VVS - 11 Years Ago
scottracing - 11 Years Ago
VVS - 11 Years Ago
carbonfibreworks - 11 Years Ago
VVS - 11 Years Ago
carbonfibreworks - 11 Years Ago
VVS - 11 Years Ago
     WOW!!!!!
redeye - 11 Years Ago
Jacopo Carbonio - 11 Years Ago
VVS - 11 Years Ago
matthieutje65 - 11 Years Ago
VVS - 11 Years Ago
matthieutje65 - 11 Years Ago
JRT - 11 Years Ago
VVS - 11 Years Ago
JRT - 11 Years Ago
VVS - 11 Years Ago
Ronny - 11 Years Ago
VVS - 11 Years Ago
redeye - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
redeye - 11 Years Ago
Ronny - 11 Years Ago
Hanaldo - 11 Years Ago
VVS - 11 Years Ago
Dravis - 11 Years Ago
VVS - 11 Years Ago
VVS - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search