learn composites in three easy steps, Race GSXR 400 build (slow)
learn composites in three easy steps, Race GSXR 400 build (slow)
Post Reply
Like
10
learn composites in three easy steps, Race GSXR 400 build (slow)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
VVS
VVS
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Moderators
Posts: 226,
Visits: 334
First off can i say none of this would happen if it it wasn't for Paul, Matt and the guys at Easy Composites,
to say you couldn't meet a nicer, more helpful, informative, interested in your project, etc, etc. bunch of people.
Paul and Matt have bent over backwards to help me and thanks have to be said.
I first went to EC at the old building to pick up a skinning kit to skin the header tank on my road bike and ended up making a rea rseat cover
can be seen in the picture
This was a bad idea and has sent me down the road of composite hell, lol
I started rebuilding an old gsxr 400 race bike and decided to replace all the old uv damaged panels in CF.
first part was the air box so I got to work.
will use tank as top of box
my first play with wax sheet and filleting wax
box fitted to bike
Edited
11 Years Ago by
VVS
Reply
Like
10
Reply
Matt (Staff)
Matt (Staff)
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 680,
Visits: 1.9K
Loving the work Chris; you've put some serious work in to get this far and it really is paying off. It's been clear from the start that you were going to go in 'at the deep end' in terms of complexity and standard of finish required - generally we advise customers to start easy and work up in order to avoid being put-off when difficult things don't go right but I'm pleased to say that you totally ignored this advice and through skill, patience and hard work will get the results anyway.
It's great to have another project so well documented on the forum and being really open and honest about problems that are encountered. The nature of composites, with so many different projects and different material combinations possible is that there is *always* an element of the unknown. You have to be prepared for some problems and persevere when they occur.
I can't wait to see and read more
--Matt
Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Tags
carbon fibre
fairings
motorbike
motorcycle
moulding
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
learn composites in three easy steps, Race GSXR 400 build (slow)
VVS
-
11 Years Ago
Started on the bodywork moulds, small pieces first, hopefully learn enough before the bigger main...
VVS
-
11 Years Ago
Looking good so far!! The rattle can problem is unfortunately a common one. You were lucky to get...
Warren (Staff)
-
11 Years Ago
Moulds are coming along nicley, and the Bike has had a new paint job Win!, Win!! looking forward to...
davro
-
11 Years Ago
Cheers davro, ive more moulds and parts done but need to find time to edit and post the pictures....
VVS
-
11 Years Ago
Having had the side panel mould go belly up and repainting the other panels i broke up the laborious...
VVS
-
11 Years Ago
Certainly doing a good job. One thing I would recommend which took me awhile to accept, is to make...
Hanaldo
-
11 Years Ago
Wow - watching in awe - those look great. I'm glad you're not being hard on yourself regarding a few...
redeye
-
11 Years Ago
Haha, those flanges are slowly getting bigger! I'm open the help, tips and criticism as learning...
VVS
-
11 Years Ago
looking good, what are you using to make the flanges with? and how easy is it to bend and conform to...
scottracing
-
11 Years Ago
Loving the work Chris; you've put some serious work in to get this far and it really is paying off....
Matt (Staff)
-
11 Years Ago
@ Scott Hi, apart from hot glue, scissors and craft knife everything is from EC. I use filleting...
VVS
-
11 Years Ago
Very clever bit of lathe work there ... excellent idea! My lathe is already running :w00t: :laugh:
Dravis
-
11 Years Ago
Its really cleaned everything up and only needs a small amount of gum to seal. machined the pipe...
VVS
-
11 Years Ago
Dravis, forgot to say center hole drilled at 5mm. Guessing you could play around with hole...
VVS
-
11 Years Ago
Yeah, I'll experiment ... then post here ... Then EC can copy them in bulk and sell them like hot...
Dravis
-
11 Years Ago
Haha, patent pending!
VVS
-
11 Years Ago
THE DOUBLE INFUSION. What can I say, I will not be doing another in a hurry! The idea was simple,...
VVS
-
11 Years Ago
Hi Chris, Infusion are looking nice! getting a bit keen with the double infusion ;) When I clear...
davro
-
11 Years Ago
Turning the pump off wouldn't have worked either, as it isn't the pump that does the infusing, it's...
Hanaldo
-
11 Years Ago
Yes having read the principle of resin being pushed in under atmospheric pressure i should know this...
VVS
-
11 Years Ago
Yes you can throttle the resin feed quite easily with a line clamp. Also for cosmetic parts you can...
Warren (Staff)
-
11 Years Ago
I will have a play about with a couple of small parts to get a feel so im better equipped for the...
VVS
-
11 Years Ago
looking good! thanks for sharing :) keep up the good work ;)
matthieutje65
-
11 Years Ago
Had to leave the bike sad and lonely for a couple of weeks due to going to Oulton Park and Anglesey...
VVS
-
11 Years Ago
For tricky little strip's of fabric like that, I suggest getting some spray adhesive from EC and...
Hanaldo
-
11 Years Ago
Yes got you mate and already there. I've purchased some FusionFix™ GP and also got some pro carbon...
VVS
-
11 Years Ago
Found a few hours so pulled the nose cone from the new mould....
VVS
-
11 Years Ago
impressive work, I might have to buy another bike just so you can make some parts for it :)
scottracing
-
11 Years Ago
Haha, still learning my trade, should have it sussed by the time I finish the bike, problem then is...
VVS
-
11 Years Ago
Very nice work :) Chris Carbon fibre works LTD
carbonfibreworks
-
11 Years Ago
Cheers Chris. If you remember we had a chat at EC one Saturday morning. Got to sort the lay ups...
VVS
-
11 Years Ago
[quote][b]VVS (16/06/2015)[/b][hr]Cheers Chris. If you remember we had a chat at EC one Saturday...
carbonfibreworks
-
11 Years Ago
Can i just say photobucket is a real pain and has a mind of its own, if the pictures are of...
VVS
-
11 Years Ago
WOW!!!!!
redeye
-
11 Years Ago
Great work :D I love photos during the process :cool:
Jacopo Carbonio
-
11 Years Ago
Thanks guys, I'm new to this so still learning, glad you like the stuff so far. I had set up to do...
VVS
-
11 Years Ago
thanks for all the great images once again! To add a little remark about the polishing of the mould,...
matthieutje65
-
11 Years Ago
That's interesting leaving the mould keyed. I think as I how some experience of working with auto...
VVS
-
11 Years Ago
The result is still better than a scotch pad with 800grid moulds. So parts are coming out of the...
matthieutje65
-
11 Years Ago
Awesome job Chris, keep it up!
JRT
-
11 Years Ago
99 Problems and a vac leak is one If you having vac problems I feel bad for you son I got 99...
VVS
-
11 Years Ago
I feel your pain brotha lol
JRT
-
11 Years Ago
Haha, I was in a dark place. If you want to make parts using composites then you will have to...
VVS
-
11 Years Ago
I feel you... Strange no one has come up with some tricks to find those leaks. How about filling it...
Ronny
-
11 Years Ago
Haha, they pretty much do supply that sort of service! Liquid would be a nono around your resin...
VVS
-
11 Years Ago
I am yet to go down the vacuum route, but the "hearing it" comment makes me wonder if making a small...
redeye
-
11 Years Ago
I have an infallible micro leak detector .. she's called Andrea and is 11 years old ... :D :w00t:...
Dravis
-
11 Years Ago
Not sure about the sniffer as i believe they don't work with the very small leaks. As you can read...
VVS
-
11 Years Ago
That looks fanfreeakingtastic! Wowzer man, well done, be proud. I have a tony little part I will...
redeye
-
11 Years Ago
[quote] finding leaks via hearing I would have a hard time explaining myself :) [/quote] Well lol...
Ronny
-
11 Years Ago
Leak detectors do work, and if you have the electrical knowledge to knock one up yourself for 30...
Hanaldo
-
11 Years Ago
I think we all need an Andrea. Hoping that with a little more experience I will get less leaks.
VVS
-
11 Years Ago
One problem is that not all micro-leaks make a sound ... :crying: so even an Andrea is not...
Dravis
-
11 Years Ago
You know it makes sense, should definitely treat it to a carbon coat.👍
VVS
-
11 Years Ago
Sorry not to have posted any of my bike build recently but i have had to leave it as ive been making...
VVS
-
11 Years Ago
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search