Hello Just curious. Why didn't you just follow the tried and proven skinning method described on this web site? You brush on the black surface coat and when almost tack free state you apply the carbon and smooth it down and apply the clear epoxy in a number of layers. When cured, you flat sand/ and 2k clear/ compound to what ever sheen you desire. Its perfect! I have done this a number of times without any problems. I am about to skin my entire airplane dash with this method. This dash has some very complex shapes. Fred
|