Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
I want to do a cosmetic skinning to my work desk, using spread-tow...
I want to do a cosmetic skinning to my work desk, using spread-tow 15mm 2/2 twill
Post Reply
Like
3
I want to do a cosmetic skinning to my work desk, using spread-tow 15mm 2/2 twill
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TDShimo
TDShimo
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 65
I would like to freshen the look of my workstation by applying a carbon fibre skin to this desktop. This application means that the carbon fibre won't need to have any structural strength, merely cosmetic. I'd like to use a large-pattern cloth, like spread-tow 15mm 2/2 twill. You can see from the photos that the desk is a boomerang shape, with a number of different curves. The dimensions of the desk are
[EDIT: Changed specs - it's larger, critically, in the max depth]
43 1/4" max depth, 88 5/8" width, and approximately 1" thick, with a few other contours shown (or, 1.1M x 2.25M x 25mm). I'd like it to have a high-gloss finish, or possibly, a nice, even matte finish with some texture. The substrate is some kind of fibre-reinforced resin. I'd like to wet lay the CF on the desktop, and wrap it around underneath just enough so it is cosmetically pleasing (though not cover the underside).
Questions:
- Is a 15mm 2/2 twill appropriate for this application (with these contours), or am I looking at a challenging application?
- How many layers would be necessary?
- Does the 0.95M + 25mm (x2) dimension present a problem with standard fabric sizes/rolls?
- Is it reasonable to expect a nice, even, glossy finish without using a mould? Or, would it be more appropriate to try for a matte finish?
- If this project is feasible, is there a kit available from Easy Composites that would be appropriate?
Thanks for your guidance!
Edited
11 Years Ago by
TDShimo
Reply
Like
3
Reply
TDShimo
TDShimo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 65
Outstanding, Dravis - that's *exactly* what I was hoping to learn (and was worried about). Thanks for your response. When you say "conform," are you talking about keeping the alignment relatively straight? And, would this be alleviated somewhat with a smaller pattern - like a 7.5mm spread tow? I love the large pattern...
... but I do like the idea of doing two patterns, with a twill on the edges. I just fear that I'll have difficulty in getting it even... having it even is more important to me than having it dead straight.
And, how many layers would you think?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
I want to do a cosmetic skinning to my work desk, using spread-tow 15mm 2/2 twill
TDShimo
-
11 Years Ago
Getting the spread tow to conform around the sharp edges at the back will probably be very...
Dravis
-
11 Years Ago
Outstanding, Dravis - that's *exactly* what I was hoping to learn (and was worried about). Thanks...
TDShimo
-
11 Years Ago
The alignment would be one difficulty, but actually getting the spread tow to stick to the table...
Hanaldo
-
11 Years Ago
As "hanaldo" writes, the difficulty is in keeping the CF spread tow to "stay in place" ... it can...
Dravis
-
11 Years Ago
Okay, so I'm not sure if any of you are still tracking this thread, but, here are the results......
TDShimo
-
10 Years Ago
Hello Just curious. Why didn't you just follow the tried and proven skinning method described on...
fgayford
-
10 Years Ago
Some sanding and recoating might give you beter results, did it on a ironman mask you can...
matthieutje65
-
10 Years Ago
What bartop epoxy did you use and where did you get it? I'm looking to use resin for a worktop as...
dmgeurts
-
10 Years Ago
fgayford - I didn't use the "tried and true" methods principally because this was the first time I...
TDShimo
-
10 Years Ago
It's by trial and error you will learn ;) but you can be proud of the results you got, it's a badass...
matthieutje65
-
10 Years Ago
[quote][b]TDShimo (02/01/2015)[/b][hr]fgayford - I didn't use the "tried and true" methods...
fgayford
-
10 Years Ago
Oh no, I no longer feel bad - just tremendously motivated and now empowered to build more stuff. But...
TDShimo
-
10 Years Ago
WOW! That looks great.The Carbon looks good in a satin finish, classy. Your doing really well. Well...
fgayford
-
10 Years Ago
Well, your skinning skills by FAR exceed my efforts. I quickly decided that skinning was not the...
Hanaldo
-
10 Years Ago
The desk still looks awesome. The skinning method using a base coat to blot out colour and stick the...
Warren (Staff)
-
10 Years Ago
Oooh, the ProFinish is what I should have been doing all along... for sure. I've been able to...
TDShimo
-
10 Years Ago
I used a product called Pro Glas 1100 from a U.S. wholesaler/retailer, Fiberlay. I don't know...
TDShimo
-
10 Years Ago
Ah, another US supplier. Being based in the UK means that most US based sources won't ship.
dmgeurts
-
10 Years Ago
That stuff is almost certainly the same as this:...
Dravis
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages