I want to do a cosmetic skinning to my work desk, using spread-tow 15mm 2/2 twill


I want to do a cosmetic skinning to my work desk, using spread-tow 15mm 2/2 twill
Author
Message
TDShimo
TDShimo
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 7, Visits: 65
I would like to freshen the look of my workstation by applying a carbon fibre skin to this desktop. This application means that the carbon fibre won't need to have any structural strength, merely cosmetic. I'd like to use a large-pattern cloth, like spread-tow 15mm 2/2 twill. You can see from the photos that the desk is a boomerang shape, with a number of different curves. The dimensions of the desk are [EDIT: Changed specs - it's larger, critically, in the max depth] 43 1/4" max depth, 88 5/8" width, and approximately 1" thick, with a few other contours shown (or, 1.1M x 2.25M x 25mm). I'd like it to have a high-gloss finish, or possibly, a nice, even matte finish with some texture. The substrate is some kind of fibre-reinforced resin. I'd like to wet lay the CF on the desktop, and wrap it around underneath just enough so it is cosmetically pleasing (though not cover the underside). 

Questions: 
- Is a 15mm 2/2 twill appropriate for this application (with these contours), or am I looking at a challenging application?
- How many layers would be necessary?
- Does the 0.95M + 25mm (x2) dimension present a problem with standard fabric sizes/rolls?
- Is it reasonable to expect a nice, even, glossy finish without using a mould? Or, would it be more appropriate to try for a matte finish? 
- If this project is feasible, is there a kit available from Easy Composites that would be appropriate?


Thanks for your guidance!

http://www.talkcomposites.com/Uploads/Images/094d3110-530c-4e3d-96e1-7b1b.png




http://www.talkcomposites.com/Uploads/Images/25e4b937-8999-47b8-9b8f-dce.jpeg

http://www.talkcomposites.com/Uploads/Images/80d8bcd4-ca86-48fb-b3c0-d3d.jpeg
Edited 11 Years Ago by TDShimo
Replies
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hello
Just curious. Why didn't you just follow the tried and proven skinning method described on this web site?
You brush on the black surface coat and when almost tack free state you apply the carbon and smooth it down and apply the clear epoxy in a number of layers. When cured, you flat sand/ and 2k clear/ compound to what ever sheen you desire. Its perfect!
I have done this a number of times without any problems. I am about to skin my entire airplane dash with this method. This dash has some very complex shapes.
Fred  
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Some sanding and recoating might give you beter results, did it on a ironman mask 

http://www.talkcomposites.com/Uploads/Images/24b86f2c-41c5-4bef-9ca9-74ad.JPG


you can find the full tutorial on here https://www.youtube.com/watch?v=oMSaPzoohHY

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TDShimo - 11 Years Ago
Dravis - 11 Years Ago
TDShimo - 11 Years Ago
Hanaldo - 11 Years Ago
Dravis - 11 Years Ago
TDShimo - 10 Years Ago
fgayford - 10 Years Ago
matthieutje65 - 10 Years Ago
dmgeurts - 10 Years Ago
TDShimo - 10 Years Ago
matthieutje65 - 10 Years Ago
fgayford - 10 Years Ago
TDShimo - 10 Years Ago
fgayford - 10 Years Ago
Hanaldo - 10 Years Ago
Warren (Staff) - 10 Years Ago
TDShimo - 10 Years Ago
TDShimo - 10 Years Ago
dmgeurts - 10 Years Ago
Dravis - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search