Greetings,

I am in the states and received my pre-preg starter kit in an unbelievably quick 2 days! 

My question is, now that the pre-pre has been room temp  (probably higher on the delivery truck) for 48 hrs, can I put it back in the fridge to extend the shelf life until I can work on the project this weekend?
Reply
BlackNDecker
BlackNDecker
Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)Supreme Being (628 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Thanks for the reply.

Currently I have the pre-preg in the refrigerator....do you think this is suboptimal (short-term) storage temperature?
Edited 11 Years Ago by BlackNDecker
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search