By BlackNDecker - 8/6/2014 3:21:52 AM

Greetings,

I am in the states and received my pre-preg starter kit in an unbelievably quick 2 days! 

My question is, now that the pre-pre has been room temp  (probably higher on the delivery truck) for 48 hrs, can I put it back in the fridge to extend the shelf life until I can work on the project this weekend?
By BlackNDecker - 8/6/2014 2:35:51 PM

Thanks for the reply.

Currently I have the pre-preg in the refrigerator....do you think this is suboptimal (short-term) storage temperature?