Questions about easycomposites pre-preg starter kit


Author
Message
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Greetings,

I am in the states and received my pre-preg starter kit in an unbelievably quick 2 days! 

My question is, now that the pre-pre has been room temp  (probably higher on the delivery truck) for 48 hrs, can I put it back in the fridge to extend the shelf life until I can work on the project this weekend?