yes it will be a single piece part... the mould will have a lot of breaks and there is no doubt its not going to be simple.

did a trial of the binnacle at weekend... typically the temp dropped for the day I attempted it so I was worried about the mould curing and slapped it under a halogen lamp.
It cured alright but at a temp that was so high I couldnt touch the mould... it melted all the cheapo paint that was under the filler in my buck and I think evaportated the release stuff so I had to destroy the buck to remove and even then the mould isnt as smooth as the buck was.
Its still not terrible and can be used as a trial for the resin infusion process and if the part I make cant be made perfect I will just make another mould of the new part after its got back to its former glory Smile















I also started putting barriers into the rear clip ready for moulding


jamesw
jamesw
Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)Supreme Being (497 reputation)
Group: Forum Members
Posts: 61, Visits: 558
Looks interesting! Are you creating a single mould for that entire rear clip? I'm not an expert and wondering how you would get the part out with all the wraparound?

James
Edited 14 Years Ago by jamesw
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Nice project, Andy. Keep us updated.

Daz, nice to hear from you too... but come on, stop teasing us and show some pics. We all know its cured now Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Daz
Daz
Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)Supreme Being (692 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Hi There

Looks a big part to do .

Im also doing some body panels and have as of last night infused the roof











I have used soric between 2 layers of carbon, so i didnt use the flow mesh

I wish i had as it took 4 1/2 hours to infuse and i did start quite late and finnished at



Also the mould has to be quite substantial as my first one didnt cut it

I know its another expense but i would bag the mold up before you use it and see if it pulls a vacume and holds it

Thats what i do now on the big parts as its a ball ache having to strip the layers out to see where its got a tiny pin hole as my biggest mold had :-(

I also spray the gel coat on know as this seems to give a much better coverage,

This is the forum to get some great tips

Keep us updated,

Daz,
Edited 14 Years Ago by Daz
andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
Hi All

Thought Id share with you the project Im doing.. its been underway for some time now and I have been liasing with easy composites for all that time.
Hopefully posting on here will allow the experts here to chirp in when they see me making mistakes Smile

Basically I have made a new design of rear clip for my Noble, I modified the clip then took a mould from it then cut the modded sections out and tried to re-make the sections in a single piece... however we had concerns due to the size of the sections that it would crack and I want it perfect so that risk is simply not acceptable.

sooooooo

I have decided to take a mould of the entire rear clip and remake it using the resin infusion method.... its a big project for me as I have never worked with carbon fibre or any kind of resin infusion method... I have however been assured I will be able to cope, and we will see Smile

I also have a few other parts to do including light pods (my new design) and a dash binacle.

Anyhow some pics of the bucks that will be used... various states of finishes but clip and binnacle are ready for polishing... going to try to do binnacle first as its a simple design and good to start with.