Hi All
Thought Id share with you the project Im doing.. its been underway for some time now and I have been liasing with easy composites for all that time.
Hopefully posting on here will allow the experts here to chirp in when they see me making mistakes

Basically I have made a new design of rear clip for my Noble, I modified the clip then took a mould from it then cut the modded sections out and tried to re-make the sections in a single piece... however we had concerns due to the size of the sections that it would crack and I want it perfect so that risk is simply not acceptable.
sooooooo
I have decided to take a mould of the entire rear clip and remake it using the resin infusion method.... its a big project for me as I have never worked with carbon fibre or any kind of resin infusion method... I have however been assured I will be able to cope, and we will see

I also have a few other parts to do including light pods (my new design) and a dash binacle.
Anyhow some pics of the bucks that will be used... various states of finishes but clip and binnacle are ready for polishing... going to try to do binnacle first as its a simple design and good to start with.