			            I do find the use of jute and flax a bit of a false economy especially if your part needs some stiffness to it.  Both are very weak fabrics compared to carbons, so any environmental credentials are wiped out because you need to use more layers and as a consequence, more harmful resins to wet out the laminate.                
			            
  				