this is the third part that comes out exactly the same and i've done 3 diff things so far.... my kitchen oven minum is 76c so i leave that 2 hours and then take it to 110c this time i added peelply on the edges but nothing... the stack is as fallowed  2 layers of pre-preg aviation no face side... ... eassycomposite unperforated release film and breather all over the mold put inside a bag and full vac... any ideas guys... this is dirving me crazy already 


Reply
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Ramping up is not just increasing the temp by 20 degrees, it is linear increase of temperature, controlled at 2 degrees/min for example. You should build or buy a purpose built oven with a temperature controller. Also, you will need the correct out of autoclave pre-pregs, otherwise you will never get pinhole free parts outside of an autoclave.

cheers,

Good luck
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
roger sbk composites - 11 Years Ago
roger sbk composites - 11 Years Ago
wozza - 11 Years Ago
morepower - 11 Years Ago
roger sbk composites - 11 Years Ago
roger sbk composites - 11 Years Ago
morepower - 11 Years Ago
matthieutje65 - 11 Years Ago
roger sbk composites - 11 Years Ago
morepower - 11 Years Ago
matthieutje65 - 11 Years Ago
morepower - 11 Years Ago
roger sbk composites - 11 Years Ago
morepower - 11 Years Ago
roger sbk composites - 11 Years Ago
roger sbk composites - 11 Years Ago
baja_patient - 11 Years Ago
roger sbk composites - 11 Years Ago
morepower - 11 Years Ago
roger sbk composites - 11 Years Ago
roger sbk composites - 11 Years Ago
roger sbk composites - 11 Years Ago
morepower - 11 Years Ago
fgayford - 11 Years Ago
combustioncraig - 11 Years Ago
roger sbk composites - 11 Years Ago
Djekouk - 11 Years Ago
roger sbk composites - 11 Years Ago
Djekouk - 11 Years Ago
     Cool design :-)
Djekouk - 11 Years Ago
morepower - 11 Years Ago
roger sbk composites - 11 Years Ago
Djekouk - 11 Years Ago
                 No problem let go on pm
roger sbk composites - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search