By roger sbk composites - 1/20/2014 3:45:58 AM

this is the third part that comes out exactly the same and i've done 3 diff things so far.... my kitchen oven minum is 76c so i leave that 2 hours and then take it to 110c this time i added peelply on the edges but nothing... the stack is as fallowed  2 layers of pre-preg aviation no face side... ... eassycomposite unperforated release film and breather all over the mold put inside a bag and full vac... any ideas guys... this is dirving me crazy already 

By roger sbk composites - 2/23/2014 6:11:05 PM

No problem let go on pm