Hi all

is it necessary to use infusion mesh on smaller parts? (< ½m2)
I suspect that it would work without,
and opposite that the resin would know about "the path of least resistance"
and not penetrate all the layers/fibres if it could flow more freely in the mesh.

How about just start with mesh the first cm´s?


http://motoform.blogspot.se

Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi, as you say you are restricted by the moulds you have. In an ideal world you should aim for the resin to travel the shortest distance, so as you say front to back is the way forward.
I would (if the mould allowed) have the spiral the full length of the front edge with the resin feed in the middle and the vac in the middle of the back edge (where the up-turn is). You could stop the mesh just short of the up-turn, so a nice simple rectangle of mesh. If you put a 50mm square of mesh and breather cloth under the vac outlet this will choke down the resin feed once in reaches the vac outlet allowing the upturn to saturate without the need for mesh. You can also leave the resin feed clamp open for a good 30-60 seconds (depending on the size of the part) after the vac is clamped off giving you a resin rich part. Because of the moulds you have you can only have a small feed spiral and the resin has a long way to travel. Even with mesh I would think it was a pretty slow infusion.

Regards Warren

Carbon Copies Ltd
Edited 12 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 12 Years Ago
Shaneer22 - 12 Years Ago
wozza - 12 Years Ago
prsw - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
prsw - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search