Hi all

is it necessary to use infusion mesh on smaller parts? (< ½m2)
I suspect that it would work without,
and opposite that the resin would know about "the path of least resistance"
and not penetrate all the layers/fibres if it could flow more freely in the mesh.

How about just start with mesh the first cm´s?


http://motoform.blogspot.se

Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi All

First off let me ask for forgiveness for my truly horrendous IT skills in regards to the image below . The green section is the infusion mesh and the white line on the right is the resin feed spiral, i also had a spiral on the vac side also. Peel ply was used and i had four layers of carbon with no leaks in the bag and pulling full vacuum. The component below the mould is one of several i have made using these moulds and infusion with mesh over the whole component. I know the mould is far from ideal due to the size of the flanges but as stated i have used these moulds without any issues. I have think the answer is going to be don't infuse from right to left and go from top to bottom if using the no mesh method but look forward to the replies, every day is a school day Smile



http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 12 Years Ago by Bartonphoenix750
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 12 Years Ago
Shaneer22 - 12 Years Ago
wozza - 12 Years Ago
prsw - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
prsw - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search