Hi all

is it necessary to use infusion mesh on smaller parts? (< ½m2)
I suspect that it would work without,
and opposite that the resin would know about "the path of least resistance"
and not penetrate all the layers/fibres if it could flow more freely in the mesh.

How about just start with mesh the first cm´s?


http://motoform.blogspot.se

Replies
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
Always use mesh from inlet into part but only to edge off part then use peel ply to vaccum side it acts as a resin break slowing down resin,which helps to saturate reienforcement.
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Shaneer22 (25/04/2013)
Always use mesh from inlet into part but only to edge off part then use peel ply to vaccum side it acts as a resin break slowing down resin,which helps to saturate reienforcement.




I also put a small piece of mesh under the vac outlet. This helps in drawing the air out of the bag/reinforcement.

Regards Warren.

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 12 Years Ago
Shaneer22 - 12 Years Ago
wozza - 12 Years Ago
prsw - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
prsw - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search