Hi all

is it necessary to use infusion mesh on smaller parts? (< ½m2)
I suspect that it would work without,
and opposite that the resin would know about "the path of least resistance"
and not penetrate all the layers/fibres if it could flow more freely in the mesh.

How about just start with mesh the first cm´s?


http://motoform.blogspot.se

Reply
prsw
prsw
Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)Supreme Being (904 reputation)
Group: Forum Members
Posts: 112, Visits: 1K
This is turning in to a good thread, and I think I know the solution to a problem I had
on a complex part, I had mesh on a tight corner and got semi-dry fibres / bridging there.
Thanks Warren.


http://motoform.blogspot.se

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 12 Years Ago
Shaneer22 - 12 Years Ago
wozza - 12 Years Ago
prsw - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
prsw - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search