Hello

guy i need help my friend wrapped me steering wheel in carbon and told used crystal resin i googled and its look like epoxy? so he sended me part and in shipment it was damages cracked in 2 places so i cleaned them and layed resin epoxy and putted tape around but what went strange that after couple layers and 48 hours i tryed to remove tape and it started to come with resin and resin started to crack how is that? now i mixed and filled with polyster resin i hope that gonna work.

i know result tommorow but thats strange why its started to crack and come out like never was attached to surface ! before laying resin like always i brushed with 280 dry paper layed nefras liquid to take out goosy surface and then layed but what i see not sticked to each other ...

anyone used that crystal resin ? is this work like normal epoxy or i need to know something? as on youtube it seems so bubbles appear after mixing.
Reply
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
yes my friend. i filled those areas with polyster resin and it seems good. now i try water paper. i hope that gonna work as epoxy started to crack. i dont get. guy who made it told all chinese use this resin. so i guess polyster? i post photo of crack and of my fix.