Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
crystal resin question
crystal resin question
Post Reply
Like
2
crystal resin question
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
guys got from his and from chinese canister photo any idea what this can be?
Reply
Like
3
Lionel
Lionel
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 12
Hi
I attempted to make a casting of a piece I made using all kinds of adhesives like Uhu and evo Stick for example, all taped up with parcel tape. What a mess! the glue and tape adhesive reacted with the chemistry of the resin mix and turned to liquidy grunge which then stuck to everything it touched. Yours sounds like a similar situation to me. Not much help maybe but it's nice to know for future you can't mix these things together.
Reply
Like
2
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
yes guys so far brushed wet paper and everything seems perfect no sign of damage i wrap in suede and do photos.
so i dont get it is polyster or epoxy and what kind of resin is that as i took it to paint shop they told its not sanded that mean resin polished...
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
maybe that's the problem "all chinese use it" :p nice it worked out with polyester, should work as well with some laminating or repair epoxy resin normally
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
i think you are correct. i guess it also could be a lesser quality epoxy and hardener.
need more info to figure this nout
CarbonFiberCreations
Reply
Like
2
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
yes my friend. i filled those areas with polyster resin and it seems good. now i try water paper. i hope that gonna work as epoxy started to crack. i dont get. guy who made it told all chinese use this resin. so i guess polyster? i post photo of crack and of my fix.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
correct me if I'm wrong Brasco but it can only be epoxy or something like that...
It can probably not be polyester, because the mixing ratio of polyester and vinylester is with a small percentage of MEKP harderner (2-3%)
Tomdesign do you maybe have some pictures? did you sand enough around the area?
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
from what i can see it is a resin for art, casting and hobby, and for jewelry . not for composite laminates per se as we would need. it's mix ratio is 2 to 1.
i was unable to find out if it is polyester or epoxy .
not sure how to clean up the mess you have either. solvent to remove any uncured resins and sandpaper to fix any delamination
or cracking defects.
scott
CarbonFiberCreations
Edited
12 Years Ago by
brasco
Reply
Like
3
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello
guy i need help my friend wrapped me steering wheel in carbon and told used crystal resin i googled and its look like epoxy? so he sended me part and in shipment it was damages cracked in 2 places so i cleaned them and layed resin epoxy and putted tape around but what went strange that after couple layers and 48 hours i tryed to remove tape and it started to come with resin and resin started to crack how is that? now i mixed and filled with polyster resin i hope that gonna work.
i know result tommorow but thats strange why its started to crack and come out like never was attached to surface ! before laying resin like always i brushed with 280 dry paper layed nefras liquid to take out goosy surface and then layed but what i see not sticked to each other ...
anyone used that crystal resin ? is this work like normal epoxy or i need to know something? as on youtube it seems so bubbles appear after mixing.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search