By TomDesign - 1/28/2013 12:18:52 PM
Hello
guy i need help my friend wrapped me steering wheel in carbon and told used crystal resin i googled and its look like epoxy? so he sended me part and in shipment it was damages cracked in 2 places so i cleaned them and layed resin epoxy and putted tape around but what went strange that after couple layers and 48 hours i tryed to remove tape and it started to come with resin and resin started to crack how is that? now i mixed and filled with polyster resin i hope that gonna work.
i know result tommorow but thats strange why its started to crack and come out like never was attached to surface ! before laying resin like always i brushed with 280 dry paper layed nefras liquid to take out goosy surface and then layed but what i see not sticked to each other ...
anyone used that crystal resin ? is this work like normal epoxy or i need to know something? as on youtube it seems so bubbles appear after mixing.
|
By TomDesign - 2/14/2013 8:43:13 PM
guys got from his and from chinese canister photo any idea what this can be?

|
|