Hello

guy i need help my friend wrapped me steering wheel in carbon and told used crystal resin i googled and its look like epoxy? so he sended me part and in shipment it was damages cracked in 2 places so i cleaned them and layed resin epoxy and putted tape around but what went strange that after couple layers and 48 hours i tryed to remove tape and it started to come with resin and resin started to crack how is that? now i mixed and filled with polyster resin i hope that gonna work.

i know result tommorow but thats strange why its started to crack and come out like never was attached to surface ! before laying resin like always i brushed with 280 dry paper layed nefras liquid to take out goosy surface and then layed but what i see not sticked to each other ...

anyone used that crystal resin ? is this work like normal epoxy or i need to know something? as on youtube it seems so bubbles appear after mixing.
Reply
Lionel
Lionel
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 4, Visits: 12
Hi

I attempted to make a casting of a piece I made using all kinds of adhesives like Uhu and evo Stick for example, all taped up with parcel tape. What a mess! the glue and tape adhesive reacted with the chemistry of the resin mix and turned to liquidy grunge which then stuck to everything it touched.  Yours sounds like a similar situation to me.  Not much help maybe but it's nice to know for future you can't mix these things together.