Carbon skinning final sand problem !!


Author
Message
Lillee
L
Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)Forum Member (36 reputation)
Group: Forum Members
Posts: 5, Visits: 25
Hey so if done some bike panels in carbon skinning the process went really well right up till final sand with 400 grit the panels have started to peel almost like orange peel on the resin, I'm now completely stuck on how to progress forward 
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
CmCarbon - 4/6/2019 11:29:26 PM
If your skinning I just use surf board poly resin. .crystal clear, higher temp rating.easy sandandcuresin 10mins if it's warm
. final coat adds me wax additive and seals and cures so it can be sanded

I personally think the XCR resin is an excellent product for skinning pieces. I don't skin that much pieces because I prefer using moulds and resin infusion or prepreg, but when skinning pieces XCR is the best resin I've tried so far. Never had problems with it so far. Just need to be sure to mix it well and use it in the correct conditions like on the TDS. 
Most important thing is to use it in a stable environment, so avoid having big temperature changes. 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lillee - 6 Years Ago
CmCarbon - 6 Years Ago
Lillee - 6 Years Ago
CmCarbon - 6 Years Ago
             Thank you very much I wil 're try
Lillee - 6 Years Ago
matthieutje65 - 6 Years Ago
Lillee - 6 Years Ago
CmCarbon - 6 Years Ago
Lillee - 6 Years Ago
CmCarbon - 6 Years Ago
matthieutje65 - 6 Years Ago
CmCarbon - 6 Years Ago
matthieutje65 - 6 Years Ago