Hello,

I have a small question...I do not have access to  a good oven for out-of-autoclave pre-preg (at least not good enough that the cycles are accurate), but I do have access to a sterilizing autoclave...

Sorry for the naive questions, but is such an autoclave OK for pre-preg ? Do you need to keep a vacuum system when using an autoclave despite the fact that there is high pressure in the autoclave itself ? Is moisture a problem (or it's OK but the part must then be put in a protective bag) ? Can someone give me a link to an autoclave protocol (temperature, time, pressure) for the use of the pre-preg in such system ? I don't think there is much indicated on the easycomposite website on that.

Thank you !!

Reply
Rakesh Verma
Rakesh Verma
Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)
Group: Forum Members
Posts: 6, Visits: 50
Damien Coudreuse - 2/6/2019 1:02:42 PM
[quote]
Damien Coudreuse - 2/6/2019 1:02:42 PM
Hello,

I have a small question...I do not have access to  a good oven for out-of-autoclave pre-preg (at least not good enough that the cycles are accurate), but I do have access to a sterilizing autoclave...

Sorry for the naive questions, but is such an autoclave OK for pre-preg ? Do you need to keep a vacuum system when using an autoclave despite the fact that there is high pressure in the autoclave itself ? Is moisture a problem (or it's OK but the part must then be put in a protective bag) ? Can someone give me a link to an autoclave protocol (temperature, time, pressure) for the use of the pre-preg in such system ? I don't think there is much indicated on the easycomposite website on that.

Thank you !!


https://xirtue.net/composite-autoclave/


Rakesh Verma
+8613861177443
vermachina@gmail.com



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search