Soft spots on the part 5 days after infision


Author
Message
KP
K
KP
posted 8 Years Ago HOT
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 2, Visits: 27
Hi.

Ok happened my fault.
I did not steer resin enough or used wrong ratio, after 5 days still have few soft spots on my part.
What can I do to fix it?
Or it cannot be fixed and i have to scrap the part.
Part das not need to look nice it is bottom part of my bonnet.

 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Initially try and use some heat to see if it will cook off.  Is it right through or just on the surface? Surface you can just gouge it off and recoat.

Patches of poorly cured resin are not usually a mixing ratio issue  -  the whole lot would likely be soft if it is.  Patches is normally poor mixing, either you didn't spend enough time mixing or did not mix it properly.  Sometimes it can be the last dregs from the mixing bucket too but that can be avoided by mixing, then pouring into a jug or similar to infuse from.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
KP
K
KP
posted 8 Years Ago HOT
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 2, Visits: 27
Hi.
Thank you for quick answer.
Hot air gun did not help much so i recoat everything with resin (mixed correctly with hardner this time).
Anyway infusion proces was very smooth thanks to your products, top part of bonnet will be next.
Any advise to infusjon this big parts will be apprecieated, bonnet is 1.7m long ad 1.6m wide.
Picture of bottom part recoatet in attachment.

My setup for top part will be:
- 2 x 220gm twill
- 2mm soric core
- 1x 220gm twill
- peelply 
- vaccum bag

Regards.


Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If you haven't already done so then i would recommend watching our video series on making a bonnet. It covers exactly what you are doing.

If the frame is reasonably stiff, then use only one layer of cloth on the surface so that your bonnet skin has a balance laminate and is less likely to warp.  Probably unlikely to be a major issue but on a good sized bonnet, you could knock things out a few mm  with warpage from an  unbalanced laminate. Usually that is within tolerance of adjustment on the latch and  hinges though.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search