Initially try and use some heat to see if it will cook off. Is it right through or just on the surface? Surface you can just gouge it off and recoat.
Patches of poorly cured resin are not usually a mixing ratio issue - the whole lot would likely be soft if it is. Patches is normally poor mixing, either you didn't spend enough time mixing or did not mix it properly. Sometimes it can be the last dregs from the mixing bucket too but that can be avoided by mixing, then pouring into a jug or similar to infuse from.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|