Carbon fiber intake plenum


Author
Message
Elias_GR
Elias_GR
Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)Supreme Being (121 reputation)
Group: Forum Members
Posts: 11, Visits: 604
Hello everyone! 

I'm planing on making an intake plenum from carbon fiber and kevlar. It is for a turbocharged car, so it needs to withstand some pressure!
The boost will be under 1 bar at the moment but I'm planning on testing the part on 3 bars at least, for reassurance.
The parts will be made from heat resistant Vinylester probably, if not Epoxy resin and vacuum infusion.

I'm planning on using 3 layers of 200gr 2X2 Twill Carbon fiber and 2 or 3 layers of hybrid 164gr Plain Carbon/Kevlar, alternatly in the layers.
By that, I mean, the first layer will be Carbon fiber, then Carbon/Kevlar, then Carbon fiber etc etc.

Will these layers and fabrics will be enough? Should I add anything or change any of the layers?

Here is the 3D model of the parts in assembly. 

http://www.talkcomposites.com/Uploads/Images/ebdd8fd4-90c6-48d1-b1f0-a5c4.JPG


http://www.talkcomposites.com/Uploads/Images/a0ec41ec-9a6e-4ba7-b162-d36f.JPG
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Interesting... CA, SR? Or something less mainstream? 

The build thread for my oven is herehttp://www.talkcomposites.com/21047/MDF-Curing-Oven?PageIndex=1 

Still working like a charm, and I'm currently considering building a second, bigger version now that I am very active with pre-preg. Definitely the way to go!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
Elias_GR - 9 Years Ago
Hanaldo - 9 Years Ago
andygtt - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 8 Years Ago
davro - 8 Years Ago
Elias_GR - 8 Years Ago
Jadleybray - 8 Years Ago
Hanaldo - 8 Years Ago
Elias_GR - 8 Years Ago
andygtt - 8 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
Hanaldo - 7 Years Ago
Elias_GR - 7 Years Ago
ArturK - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search