Sanding my parts and it's looking like this? How to fix?


Author
Message
deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Sanding my parts and it has like a billion low spots to it. Any idea why it is doing this and how to fix? 

http://www.talkcomposites.com/Uploads/Images/bd479931-9f38-48a7-a2dd-086e.jpghttp://www.talkcomposites.com/Uploads/Images/8ab24f0d-67a4-49a4-85c4-713a.jpg
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I use this same resin for resin coating and it's good for that. 

Just keep applying coats while the resin green and not fully cured. This way you can build 2-3 coats without sanding in-between and all in the one day. Then hopefully sand it only once! then spray coat with any other UV clear coat you like.