Sanding my parts and it's looking like this? How to fix?


Author
Message
deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Sanding my parts and it has like a billion low spots to it. Any idea why it is doing this and how to fix? 

http://www.talkcomposites.com/Uploads/Images/bd479931-9f38-48a7-a2dd-086e.jpghttp://www.talkcomposites.com/Uploads/Images/8ab24f0d-67a4-49a4-85c4-713a.jpg
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Sand, spray clear coat, repeat. 