Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Sanding my parts and it's looking like this? How to fix?
Sanding my parts and it's looking like this? How to fix?
Post Reply
Like
3
Sanding my parts and it's looking like this? How to fix?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
deceased10
deceased10
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 29,
Visits: 154
Sanding my parts and it has like a billion low spots to it. Any idea why it is doing this and how to fix?
Reply
Like
3
Reply
deceased10
deceased10
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 29,
Visits: 154
So is this normal then? Or is that a sign of sanding through to the carbon fibre? I put two thick coats on
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Sanding my parts and it's looking like this? How to fix?
deceased10
-
9 Years Ago
Sand, spray clear coat, repeat.
Hanaldo
-
9 Years Ago
You could also use the EC skinning resin and this will give the parts a thick coat of clear then...
carbonfibreworks
-
9 Years Ago
So is this normal then? Or is that a sign of sanding through to the carbon fibre? I put two thick...
deceased10
-
9 Years Ago
So is this normal then? Or is that a sign of sanding through to the carbon fibre? I put two thick...
deceased10
-
9 Years Ago
I'm assuming this part is skinned? 100% normal for parts not made in a mould.
Hanaldo
-
9 Years Ago
You have not said what your process is so far? Looks like a wet layup and maybe one further coat of...
Fasta
-
9 Years Ago
Sorry should of mentioned that. This is a skinned part. I am using west systems epoxy 205 resin 207...
deceased10
-
9 Years Ago
I wouldn't use west for skinning parts,from my experience,your better off using sp 320.
Shaneer22
-
9 Years Ago
Nothing wrong with West System for skinning. There's better resins for sure, but it's ok for the...
Hanaldo
-
9 Years Ago
Yeah Unfortunately not to many epoxys available in my area. Even had to order this epoxy online....
deceased10
-
9 Years Ago
I use this same resin for resin coating and it's good for that. Just keep applying coats while the...
Fasta
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search