Sanding my parts and it has like a billion low spots to it. Any idea why it is doing this and how to fix? 

http://www.talkcomposites.com/Uploads/Images/bd479931-9f38-48a7-a2dd-086e.jpghttp://www.talkcomposites.com/Uploads/Images/8ab24f0d-67a4-49a4-85c4-713a.jpg
Reply
deceased10
deceased10
Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)Supreme Being (215 reputation)
Group: Forum Members
Posts: 29, Visits: 154
Yeah Unfortunately not to many epoxys available in my area. Even had to order this epoxy online. Gonna stick with it. Hanaldo thanks for the tips Ill do that! 