hello guys 
new member here Smile
i want to make some structural assemblies from pre-preg cf and i wonder if easycomposites cf is strong enough , or is it just for show purpose / body panels use only ?
for example , when i compare resin properties to cycom 2020 which is used in formula 1 etc i see big difference , but the measurements were made on different systems (iso and astm)

i added the mechanical properties , so how those two can be compared ?



easycomposites :

http://www.talkcomposites.com/Uploads/Images/bd3c2d6c-9f26-4d64-9d58-8268.jpg

cytec cycom 2020 :
http://www.talkcomposites.com/Uploads/Images/19d7cddf-2255-4030-8b99-43ba.jpg



Reply
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
You can,but very slowly increase tempreture so parts does not deform.i have post cured unimold upto 120.