one more question ...
if i want to cure @130c , the mold materials can hold up to 80c only , can i continue curing the part after de-molding ?
thanks
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
You can,but very slowly increase tempreture so parts does not deform.i have post cured unimold upto 120.
creator
creator
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 9, Visits: 92
Sorry, 
You have post cured a part with a unimold mandrel
Or you have used the unimold at curing scedule up to 
120 Celsius with out deformation? 