By sss
-
12/26/2014 11:24:33 AM
hello guys
new member here
i want to make some structural assemblies from pre-preg cf and i wonder if easycomposites cf is strong enough , or is it just for show purpose / body panels use only ?
for example , when i compare resin properties to cycom 2020 which is used in formula 1 etc i see big difference , but the measurements were made on different systems (iso and astm)
i added the mechanical properties , so how those two can be compared ?
easycomposites :
cytec cycom 2020 :
By creator
-
4/18/2015 8:02:01 AM
Sorry,
You have post cured a part with a unimold mandrel
Or you have used the unimold at curing scedule up to
120 Celsius with out deformation?