Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Few carbon parts for Noble M12
Few carbon parts for Noble M12
Post Reply
Like
3
Few carbon parts for Noble M12
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
andygtt
andygtt
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
Hi All
Thought Id share with you the project Im doing.. its been underway for some time now and I have been liasing with easy composites for all that time.
Hopefully posting on here will allow the experts here to chirp in when they see me making mistakes
Basically I have made a new design of rear clip for my Noble, I modified the clip then took a mould from it then cut the modded sections out and tried to re-make the sections in a single piece... however we had concerns due to the size of the sections that it would crack and I want it perfect so that risk is simply not acceptable.
sooooooo
I have decided to take a mould of the entire rear clip and remake it using the resin infusion method.... its a big project for me as I have never worked with carbon fibre or any kind of resin infusion method... I have however been assured I will be able to cope, and we will see
I also have a few other parts to do including light pods (my new design) and a dash binacle.
Anyhow some pics of the bucks that will be used... various states of finishes but clip and binnacle are ready for polishing... going to try to do binnacle first as its a simple design and good to start with.
Reply
Like
3
Reply
andygtt
andygtt
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
Started to make the inner panels for the rear clip... I was going to remake them but decided it wasnt worth the extra work as they are only functional and MAY be coated in an underseal. Unlike original panel Im going to give them a large return and bond them in so that the rear spoiler actually bolts through it, should be massively stronger and yet not add much weight into the clip.
First task was to remove the original underseal... this job was an absolute joy lol
Anyhow after a quick sand I painted them in a 2 pack paint, sanded them back again and repainted them.. hope to start applying gel coat tomorrow after a few return barriers to allow bagging.
Pic is a little boring so I added one of the new spoiler I bought lol
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Few carbon parts for Noble M12
andygtt
-
13 Years Ago
Hi There Looks a big part to do . Im also doing some body panels and have as of last night infused...
Daz
-
13 Years Ago
Nice project, Andy. Keep us updated. Daz, nice to hear from you too... but come on, stop teasing...
Joe
-
13 Years Ago
Looks interesting! Are you creating a single mould for that entire rear clip? I'm not an expert and...
jamesw
-
13 Years Ago
yes it will be a single piece part... the mould will have a lot of breaks and there is no doubt its...
andygtt
-
13 Years Ago
Daz... Im interested in seeing a few pics of your project, maybe share a few ideas, do you have a...
andygtt
-
13 Years Ago
Hi , I havnt got a thread im waiting to finnish all the carbon and then do a build thread, One...
Daz
-
13 Years Ago
[quote][b]Daz (03/04/2012)[/b][hr]Hi , One other tip i have is when you make the molds make the...
andygtt
-
13 Years Ago
The binnacle took 3 days to cure lol... anyhow even though the bag lost pressure and the small...
andygtt
-
13 Years Ago
started laying up the mould for rear clip... huge part, loads of release lines. started with the...
andygtt
-
13 Years Ago
mould of rear clip is taking more time than I expected... It took 7 hours to do the final filler...
andygtt
-
13 Years Ago
Happy to see things going forward ! Keep us updated ;)
Joe
-
13 Years Ago
unfortunatelly an area around the number plate reacted behind the gel coat... I looked at it the...
andygtt
-
13 Years Ago
I used to make molds from parts but maybe not as big as what you've taken on. I ended up spraying...
Ragece
-
13 Years Ago
I will definatelly have to look into getting some of that polyester paint... have you used it with...
andygtt
-
13 Years Ago
Hi, I use polyester filler (2pack) as the coat on which the mold is built. It can be polished to a...
Joe
-
13 Years Ago
Pulled the mould from the buck tonight, please to say it came apart without issue :) Will check on...
andygtt
-
13 Years Ago
Nice mould and good job! did you planed to make all this part in visible carbone frame? this will...
SebRS
-
13 Years Ago
some parts will be visable carbon and I intend to have a strip over the body in raw carbon with...
andygtt
-
13 Years Ago
Good project. I read this topic since the begining, i must say i'm really fan of your project!...
SebRS
-
13 Years Ago
My noble has well over 600bhp... soon to be over 700bhp... it weights 1110kgs full of fuel (hoping...
andygtt
-
13 Years Ago
Fantastic! what amazing cars you have! you may be a bit crazy to drive this rocket on road, but i...
SebRS
-
13 Years Ago
this is one of the few videos I have... not very good I admit....
andygtt
-
13 Years Ago
Haha, nice to see things going forward ;)
Joe
-
13 Years Ago
Looking good! Diolen will add some impact resistance. The team at EC experimented with using a foam...
Warren
-
13 Years Ago
thought about foam core, but Im not sure how you apply it with the resin infusion... can I just lay...
andygtt
-
13 Years Ago
[quote][b]andygtt (02/05/2012)[/b][hr]thought about foam core, but Im not sure how you apply it with...
Warren
-
13 Years Ago
[quote][b]Warren (02/05/2012)[/b][hr][quote][b]andygtt (02/05/2012)[/b][hr]thought about foam core,...
andygtt
-
13 Years Ago
Looking good :)
Daz
-
13 Years Ago
Hi Andy Fabulous job you have done on this so far, makes my small stint in this type of work look...
JohnH
-
13 Years Ago
[quote][b]JohnH (02/05/2012)[/b][hr]Hi Andy Fabulous job you have done on this so far, makes my...
andygtt
-
13 Years Ago
use too much bag rather than too little. You will spend on a mould that size probably a good hour or...
Warren
-
13 Years Ago
what about the peel ply... can that be baggy just making sure it covers and has no voids... or does...
andygtt
-
13 Years Ago
[quote][b]andygtt (04/05/2012)[/b][hr]what about the peel ply... can that be baggy just making sure...
Warren
-
13 Years Ago
pics of progress last night...
andygtt
-
13 Years Ago
spoke to matt and he gave me the same advise... the bag is massive, I pulled a vacume yesterday but...
andygtt
-
13 Years Ago
With the fact you have soric and mesh, you shouldnt have problems with the resin not wetting out as...
Warren
-
13 Years Ago
I've enveloped bagged... not gone well, spent all day chasing leaks, I missed a few sharp edges on...
andygtt
-
13 Years Ago
You could try taping some breather fabric or similar over the joins on the underside where any...
Warren
-
13 Years Ago
i had the same problem with my first split mould, i had some advice from here to say that he used...
neilb
-
13 Years Ago
to stop any sharps on the back of my molds i have used roofing flashing tape It is self adhesive...
Daz
-
13 Years Ago
cheers for the tips.... I managed to cobble together a bag from the bagging materials I had left,...
andygtt
-
13 Years Ago
this is the back of one of my molds smooth asa babys bum...
Daz
-
13 Years Ago
This is an absolutely fantastic read Andy. Been checking for updates daily, and this is my first...
pk_090
-
13 Years Ago
Ok so time for an update.. dispite the disaster of the bag loosing pressure I went into damage...
andygtt
-
13 Years Ago
Thats turned out great despite the problems you had,
Daz
-
13 Years Ago
Bloody good work! Some people keep the pump on all the time anyway, so if it can hold a vacuum...
Warren
-
13 Years Ago
I just thumbed through your thread and I must say that you did a great job!!!! Glad to see that you...
turbodunn
-
13 Years Ago
FANTASTIC!!! just looks as profesional as it can be! Regards, Seb.
SebRS
-
13 Years Ago
Awesome !!
Joe
-
13 Years Ago
I love this project.. the way you mould it is great Cheers from Indonesia
Leon
-
13 Years Ago
I love this project.. the way you mould it is great Cheers from Indonesia
Leon
-
13 Years Ago
My car has stripes over it and these are going to be in laquered carbon... this is easy on the rear...
andygtt
-
13 Years Ago
Normal 0 false false false MicrosoftInternetExplorer4...
Matt (Staff)
-
13 Years Ago
[quote][b]Matt (Staff) (16/05/2012)[/b][hr] your project is inspiring a lot of people. [/quote] I'm...
Element6
-
13 Years Ago
Thanks Matt, thats praise indeed :cool: Must say a huge amount of the success I have had is the...
andygtt
-
13 Years Ago
Oh and thanks for all the positive comments from everyone.
andygtt
-
13 Years Ago
Started to make the inner panels for the rear clip... I was going to remake them but decided it...
andygtt
-
13 Years Ago
[IMG]http://i556.photobucket.com/albums/ss7/andy_gtt/CIMG2291.jpg[/IMG]
andygtt
-
13 Years Ago
looks awesome on the car!!
Warren
-
13 Years Ago
That is fantastic! Are you going to paint or justLacquerit Andy? Alex
pk_090
-
13 Years Ago
car will be painted however my stripes over it will be raw laquered carbon.
andygtt
-
13 Years Ago
Not to bump an old thread or owt but.... I work at the place that makes the carbon fibre bodies for...
CarbonMike
-
13 Years Ago
Coming on really good,are you making your own intake ie. air box.
Shaneer22
-
13 Years Ago
In my experience if s*** can go wrong, well it goes wrong. I'm astounded how you're able to pull it...
aza993a
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search