Mould gel coat - it set before I could apply the putty


Author
Message
Nitch
Nitch
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Hi,

I prepared and coated the original part with gel coat but got called away before getting to apply the putty at the tacky stage.  The gel coat has now gone hard.

Is there anything I can do to make the gel coat and putty now bond?

Thank you very much,

Nick
Reply
Nitch
Nitch
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Thank you for the replies guys.

This is an epoxy gel.