Hi,

I prepared and coated the original part with gel coat but got called away before getting to apply the putty at the tacky stage.  The gel coat has now gone hard.

Is there anything I can do to make the gel coat and putty now bond?

Thank you very much,

Nick
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you can brush on some acetone with a cloth or so to make it a bit tacky again... otherwise sand it with a heavy 80grid sandpaper to create a good bond again.
maybe other members have other tricks.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Is this epoxy or polyester? 
Nitch
Nitch
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Thank you for the replies guys.

This is an epoxy gel.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Hmm. The epoxy gelcoats that I use HAVE to be reinforced during the tacky stage, if you let it dry nothing will bond to it and it needs to be scraped off the mould. I Iran get away with it with my polyester gelcoats, but not the epoxies. But I use Airtech stuff, the EC stuff may be more forgiving? 
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If its our green goo and putty then sand back like Matthieu said.  It can help to add another thin layer of epoxy gel or even epoxy laminating resin as a coupling coat. 

If it hasnt gone fully hard, just lost its tack, then you can normally get away with just another thin layer of epoxy as above.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search