Hmm. The epoxy gelcoats that I use HAVE to be reinforced during the tacky stage, if you let it dry nothing will bond to it and it needs to be scraped off the mould. I Iran get away with it with my polyester gelcoats, but not the epoxies. But I use Airtech stuff, the EC stuff may be more forgiving?
|