If its our green goo and putty then sand back like Matthieu said. It can help to add another thin layer of epoxy gel or even epoxy laminating resin as a coupling coat.
If it hasnt gone fully hard, just lost its tack, then you can normally get away with just another thin layer of epoxy as above.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|