Finished the next part for project Fiesta St, the engine cover. As with the door mirrors this is a skin that will be bonded onto the original cover. The original cover has a brushed aluminum badge but the customer just wanted a ghost of the badge on the new part. Just for a changed I decided to use 450grm as the surface layer again with GC50 Gelcoat.