Finished the next part for project Fiesta St, the engine cover. As with the door mirrors this is a skin that will be bonded onto the original cover. The original cover has a brushed aluminum badge but the customer just wanted a ghost of the badge on the new part. Just for a changed I decided to use 450grm as the surface layer again with GC50 Gelcoat.

Warren







Carbon Copies Ltd
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Looks good, agreed, I much prefer the chunkier look of 450 as a surface layer