Look what happened to the gel coat :(


Author
Message
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
http://img442.imageshack.us/img442/6315/vgyz.jpg

Apparently this occured during the shipping but the package was ok and I suspect others reasons :

- Could it be due to the fact I left the gel coat (EC GC50) cure too long (more than 24hrs), causing delamination ?

- Or would it be because of the GC50 thickness (but does not seem too thick for me) ?

any other clue ?

feel bad right now Unsure 
frustrated cause the part was ok when I sent it.
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
SmileSmileSmileSmile The invoice is in the post Wink

Carbon Copies Ltd
Edited 12 Years Ago by wozza
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Warren (Staff) - 12 Years Ago
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
wozza - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search