It would need to be a chopped strand mat which is powder bound.
It would be very difficult to infuse properly as the unwetted CSM is stiff so hard to get into awkward shapes. Generally CSM is wetlay so as you put resin on it, it soaks in and the CSM goes floppy.
I would suggest you use soric. The part will be lighter and stiffer. If you want to add more layers than just the CF then woven glass is the way forward.