Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Resin Infusion
Is Chopped Strand Mat compatible with resin infusion ?
http://www.talkcomposites.com/Topic6108.aspx
By Jess8bit
-
5/16/2013 9:58:22 AM
...or do we have to use woven glass instead ?
I need to make a thick part (3mm) so I plan to use 2 layers of 195g 2/2 twill CF, and then the rest with glass (or maybe Soric ? or combination of Soric + galss ?)
thank you
J
By Jess8bit
-
5/17/2013 8:54:38 PM
Great advice Carbon Cactus, about the symmetry, it's good to have it reminded
, I tend to forget how important it is, depending on the shape.
I would also rotate the CF by 90° each, to help to prevent from warping.
I don't plan to use infusion polyester, so I think I'll do the way you propose. This stack sounds really good to me (I would have tried with woven glass, though, if I had some).
Will definitely post a picture of the final part, if I succeed
!
thanks, again.
J.