Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Is Chopped Strand Mat compatible with resin infusion ?
Is Chopped Strand Mat compatible with resin infusion ?
Post Reply
Like
4
Is Chopped Strand Mat compatible with resin infusion ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jess8bit
Jess8bit
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
...or do we have to use woven glass instead ?
I need to make a thick part (3mm) so I plan to use 2 layers of 195g 2/2 twill CF, and then the rest with glass (or maybe Soric ? or combination of Soric + galss ?)
thank you
J
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Is Chopped Strand Mat compatible with resin infusion ?
Jess8bit
-
13 Years Ago
It would need to be a chopped strand mat which is powder bound. It would be very difficult to...
Warren (Staff)
-
13 Years Ago
Thank you Warren, I only have CSM emulsion bound in stock (the one I use with Uni Mould, as EC...
Jess8bit
-
13 Years Ago
Emulsion bound and epoxy is a deffinite no go. I might be wrong but if you use a core material, it...
carboncactus
-
13 Years Ago
Great advice Carbon Cactus, about the symmetry, it's good to have it reminded :), I tend to forget...
Jess8bit
-
13 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search