Chris Rogers - 5/22/2020 6:02:13 PM
You can also cast-in-place sanding blocks with some packing tape on your surface, some polyester filler (Bondo) to take the surface shape and a wood backer to hold on to...

I'm a big fan of the 3M yellow foam blocks and the Stickit paper too - the blocks are hard enough yet have some give.  Not cheap but a great system.

You can also glue acrylic sheet to softer foam to make a flexible-yet-hard block for curved surfaces.  You want to sand (fair) with something that takes the shape of the surface you want to achieve - but no more - so you hit the high spots but don't over-sand the low ones.

Lot of ideas, thank you!

Chris Rogers
C
Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)Supreme Being (1.3K reputation)
Group: Forum Members
Posts: 120, Visits: 933
You can cast-in-place sanding blocks with some packing tape on your surface, some polyester filler (Bondo) to take the surface shape and a wood backer to hold on to...

I'm a big fan of the 3M yellow foam blocks and the Stickit paper too - the blocks are hard enough yet have some give.  Not cheap but a great system.

You can also glue acrylic sheet to softer foam to make a flexible-yet-hard block for curved surfaces.  You want to sand (fair) with something that takes the shape of the surface you want to achieve - but no more - so you hit the high spots but don't over-sand the low ones.




Edited 6 Years Ago by Chris Rogers
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 5/20/2020 12:17:05 PM
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Thank you, I will have a look at them!

Lester Populaire
L
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

Lester Populaire
L
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
scottracing - 5/20/2020 11:22:47 AM
if you are sanding specific geometry you can 3d print the blocks, allowing for an offset for the double sided tape and sand paper.

Currently just using a whole load to sand some carbon wheels, also if you are looking to buy some sanding blocks i can reccomend the perma-grit tools that easy composites sell.

Thanks Scottracing for the 3d print hint!

I already have the permagrits, unfortunately they stop at a quite coarse grits. Fantastic tools though!

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
if you are sanding specific geometry you can 3d print the blocks, allowing for an offset for the double sided tape and sand paper.

Currently just using a whole load to sand some carbon wheels, also if you are looking to buy some sanding blocks i can reccomend the perma-grit tools that easy composites sell.
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Warren (Staff) - 5/18/2020 4:28:46 PM
There are plenty of sanding blocks on the market.  You can even make your own carved from a stiff foam (or even wood).  Sometimes if you have a fixed shape a custom block can be useful.  

Thank you!

Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There are plenty of sanding blocks on the market.  You can even make your own carved from a stiff foam (or even wood).  Sometimes if you have a fixed shape a custom block can be useful.  

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search