How do you make your sand blocks?


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, what do you use as sand blocks for fairing?
I watched some tutorials but they were all about wood working. Wonder if there is some adjustment specific for composites.
So...
Wood (btw, with or without pads)?
Foam? Xps would be ok
Commercial available? Ifound permagrit blocks fantastic but they only make the coarser grits.

Thanks
Replies
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Lester Populaire - 5/20/2020 12:17:05 PM
Massimiliano - 5/20/2020 11:56:00 AM
Lester Populaire - 5/20/2020 11:53:24 AM
yes i can highly recommend the 3d printed sanding blocks for specific geometries. i mostly use PETG as it is easy to print but a little more temperature resistant than PLA. And often you can just sand a profile into a junk of MDF on the belt sander and it does the same job.

Thank you Lester!
I don't own a 3D printer but considering to buy one.
Any recommendation?

I use Prusa printers privately and at work and only had good experiences with them. There are a lot cheaper printers that work well too but they are more of a toy than a tool i feel like. The Prusas are like the the cheapest option for a reliable workhorse.

Thank you, I will have a look at them!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
             Thanks a lot!!
mporta71 - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you!
mporta71 - 5 Years Ago
scottracing - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
                     Thank you, I will have a look at them!
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago
             Lot of ideas, thank you!
mporta71 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search